质量指标
项 目
|
API 5L
|
GB/T9711.1-1997
|
SY/T5037-92
|
|||
管端外径偏差
|
+1.59mm
-0.79mm
|
D<273.1mm
|
+1.59mm
|
D<508mm
|
±0.75%D
|
|
-0.40mm
|
||||||
D≥323.9mm
|
+2.38mm
|
D≥508mm
|
±0.50%D
|
|||
-0.79
|
||||||
壁厚偏差
|
D<457.2mm
|
+15.1%t
|
D≤457mm
|
+15.0%t
|
D<508mm,±12.5%t
D≥508mm,±10.0%t
|
|
D≥508mm
|
-12.5%t
|
|||||
-12.6%t
|
+17.5%t
|
(L175,L210,L245)
|
||||
D>508mm
|
+14.5%t
|
-10.0%t
|
||||
D≥508mm
|
|
|||||
-8.0%t
|
+19.5%t
|
|||||
-8.0%t
|
||||||
直度
|
≤0.2%L
|
≤0.2%L
|
≤0.2%L
|
|||
椭圆度
|
D>508mm,± 1.0%D
|
D>508mm,± 1.0%D
|
± 1.0%D
|
|||
管端状态
|
坡口:30°~35° 钝边:1.59±0.79mm 切斜:<1.59mm |
坡口:30°~35° 钝边:1.59±0.79mm 切斜:<1.59mm |
坡口:30°~35° 钝边:1.6±0.8mm 切斜: D<813mm,≤1.5mm D≥813mm,≤3.0mm |
|||
无损检验
|
100%X射线或100%超声波加管端X射线 检验 |
100%X射线或100% 超声波加管端X射线 检验 |
补焊焊缝,对头焊缝及环
向焊缝无损检验
|
|||
水压试验
|
p=2st/D
D<508mm, s=0.85σs
D≥508mm, s=0.90σs
|
p=2st/D
L290~L555
D=219.1mm,s=0.75Rt0.5
273.1<D≤457mm,S=0.85Rt0.5
|
P=2[σ]t/D
[σ]=(0.6~0.8)σS
|
|||
备注:
|
D--钢管公称外径,mm; t--钢管公称壁厚,mm; S,[б]--水压试验应力,MPa; P--水压试验压力,MPa; σs-屈服强度Mpa; L--单根钢管长度,m; б0.5--试样标距长度上产生0.5的总伸长时所需的拉应力,MPa |
点击返回查看产品:螺旋焊管